Stainless steel drinkware material selection | ZILOOP
The three grades you will be quoted
| Grade | Nickel | Molybdenum | Relative cost | Typical use |
|---|---|---|---|---|
| SUS304 (18/8) | 8–10.5% | — | Baseline | Standard drinkware |
| SUS316 | 10–14% | 2–3% | +15–25% | Salt exposure, marine, premium |
| SUS201 | 3.5–5.5% | — | −10–15% | Low-cost outer shells |
Most drinkware uses 304 for the inner wall (food contact) and 201 or 304 for the outer shell. That combination is legitimate and common — but it must be stated, not implied.
When 316 is worth the premium
316 resists chloride attack better than 304. It matters for: coastal markets, salt-water use, and buyers who run aggressive cleaning regimes.
For inland markets with normal use, 304 is sufficient and the premium buys little.
How to verify the grade
- Mill certificate — states the heat number and composition; request it for the coil used
- XRF or spectrometer test — non-destructive, takes seconds, shows nickel and molybdenum content
- Magnetic test — 304 is weakly magnetic after forming, 201 more so; useful only as a rough screen
Ask for the XRF result on the production lot, not the sample.
Cost conversation
Grade is one of four cost drivers alongside wall thickness, finish and lid complexity. A buyer who fixes the grade but ignores wall thickness often ends up with a heavier, more expensive product than intended.
Related: 316 bottle, all drinkware.
---